UV表面自干移印油墨

服务区域:上海/嘉定/嘉定工业区
价格:230 元/千克
UV表面自干移印油墨
产品特点
(1)出色的附着力和印刷适性
(2)对各种塑料基材均有出色的附着力
(3)印刷机上的操作稳定,胶印适性出色
品牌: 欧莱斯
包装: 1KG/罐  12公斤/箱 
颜色: 红、黄、蓝、黑、白、金红、大红
 

产品特点
(1)出色的附着力和印刷适性
(2)对各种塑料基材均有出色的附着力
(3)印刷机上的操作稳定,胶印适性出色
适用范围
此款欧莱斯金属印刷UV丝印移印油墨适用于不锈钢 、光面不锈钢、金属、玻璃陶瓷等基材。

使用方法:
1.建议用我公司专用稀释剂进行稀释,不建议使用783慢干稀释剂稀释,使用前应充分搅拌,用后随时密封。
2.搅拌时加本公司配套**10-12%,稀释到印刷适合粘度,移印稀释使用移印专用稀释剂;用718洗网水清洗。
3.不得与其它类型油墨混合使用,否则容易出现其他附着力,化学反应等不良现象。
4. 加入固化剂的油墨使用时限为8小时,过期请弃用,剩余油墨不可回收
注意事项:
1.各种承印物料的外观相似,但可能会是不同的材料,客户需先试印,确其符合要求后,再批量生产。
2.在移印过程中,如出现拉丝或散开,可适当加入一些慢干膏即可;
3.环境温度过高,将会影响油墨原有质量。白色超越150都会变色,烘烤时请用木质材料垫底进行烘烤,不得直接接触铁
4.根据气候变化,请远离火源,阴暗处15度-30度环境下存放Product i n f ormation
Name: oleser stainless steel UV series ink
Brand: Brand Name:
Packing: 1KG/ 12 kg / box
Color: red, yellow, blue, black, white, red, red
Product features
(1) excellent adhesion and printing
(2) excellent adhesion to all kinds of plastic substrates
(3) the operation of the printing press is stable and the offset is good.
Scope of application
The Las Olas metal printing UV silk screen printing ink is suitable for stainless steel, polished stainless steel, metal, glass, ceramics and other substrates.
usage method:
1 rec o mmended to use my c o mpany‘s special diluent dilution, do not rec o mmend the use of 783 slow dry dilution dilution, before use should be fully stirred, sealed at any time after the.
2. Mixing Cabern e t c o mpanies supporting open water10-12% and dilution to printing for viscosity, printing the dilution used printing special thinner; with 718washing n e t w ork water cleaning.
3 shall not be mixed with other types of ink, or else it is prone to other adhesion, chemical reactions and other undesirable phenomena.
4 add hardener inks use time limit for 8 hours, please not expired, the remaining ink Unrecyclable
Matters needing attention:
1. All kinds of printing material similar in appearance, but may be of different materials, customers need to try printing and ensure its requirements, and then bulk production.
2 in the printing process, such as drawing or spread out, may be appropriate to add some slow dry paste;
3 ambient temperature is too high, will affect the quality of the original ink. More than 150 white will change color when baking, please use woodiness material bottom baking, not in direct contact with iron
4 ac c ording to climate change, please stay away from the fire source, dark place 15 degrees -30 degrees under the environment
发布时间:2024-01-15 11:03:07
联系电话:18184507496 代莉